Abstract
Abstract
Background
To assess the relationship between mechanical wear and the failure of the internal lengthening mechanism in retrieved MAGnetic Expansion Control (MAGEC) growing rods.
Methods
This study included 34 MAGEC rods retrieved from 20 patients. The state of the internal mechanism and mechanical wear were assessed in all the rods using plain radiographs and visual inspection. Metrology was then performed to assess the topography and mechanical wear of the telescopic bars, using a Talyrond 365 (Taylor Hobson, Leicester, UK) roundness measuring machine.
Results
Plain radiographs showed evidence of a broken internal mechanism in 29% of retrieved rods. Single-side wear marks were found in 97% of retrieved rods. Material loss was found to significantly increase in rods with a damaged internal mechanism (p < 0.05) and rods with longer time in situ (r = 0.692, p < 0.05).
Conclusions
We found an association between damage to the internal mechanism of the rods and (1) patterns of single-side longitudinal wear marks and (2) increased material loss. As the material loss was also found to increase over time of rod in situ, we emphasise the importance of early detection and revision of failed MAGEC rods in clinical practice.
Publisher
Springer Science and Business Media LLC
Subject
Orthopedics and Sports Medicine,Rheumatology
Cited by
10 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献