Abstract
Diamond thin films of different structures were prepared by using chemical vapor deposition on WC(6%Co) substrates under different conditions.Reman spectroscopy was used for the quality evaluation of the diamond films.The cracking size in indentation tests was used for the evaluation of adhesion strength,and the influence of structure of diamond films on the adhesion was studied.Results obtained show that: (1) The buffer role of sp2_carbon between grain boundaries greatly affect the residual stress of the film,hence the cracking size decreases steadily with increasing sp2 content.(2) The increase of nucleation density is mainlyh due to the contribution of the diamond seed grains left. In this case,the increase of nucleation density cannot effectively improve the chemical adhesioe force between the film and the WC substrate,and cannot improve the adhesion between the film and the substrate.(3)For thinner films there is no compressive stress among diamond grains,hence the cracking size does n t increase apparently with increasing deposition time.Strong compressive stress emerges only after the thickness increases to a certain value,and then the cracking size increases rapidly with increasing deposition time.
Publisher
Acta Physica Sinica, Chinese Physical Society and Institute of Physics, Chinese Academy of Sciences
Subject
General Physics and Astronomy
Cited by
10 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献