Abstract
Silicon nitride (SiNx), an important material used as a dielectric layer and passivation layer in thin film transistor liquid crystal display (TFT LCD) was patterned by a non-lithographic process. SiNx was deposited by plasma enhanced chemical vapor deposition (PECVD) on glass substrate. Laser photoablation can effectively pattern 5 µm diameter with 200 nm depth hole in SiNx thin films with laser photoablation. The threshold remove fluence is 1350 mJ/cm2 with 1 laser irradiation shot. The contact-hole taper angle as a function of the laser irradiation shot number. The taper angle increased with increasing the laser irradiation shot number. The contact-hole taper angle etched profile was successfully controlled by vary the laser irradiation shot number.
Publisher
Trans Tech Publications, Ltd.
Reference9 articles.
1. Dirk Basting, Excimer laser technology: systems and applications, publication by lambda physic, (2001) 145.
2. J. Ihlemann; B. W. Rottke, Appl. Surface Sci., 106 (1996) 282.
3. J.E. Andrew; P.E. Dyer; R.D. Greenough; P.H. Key, Appl. Phys. Lett., 43 (1983) 11.
4. Q. Yavas; M. Takai, Jpn. J. Appl. Phsy., 38 (1999) 7131.
5. J. Chae; S. Appasamy; K. Jain, Appl. Phsy. Lett., 90 (2007) 261102.
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献