Abstract
Diluted magnetic semiconductor Zn1-xMnxO crystals were synthesized at 430°C for 24h by hydrothermal method. 3mol·L-1KOH was used as the mineralizer, and the fill factor is 35%. The obtained crystals show a ZnO wurtzite structure, with positive polar faces{0001}, negative polar faces{000 }, p faces{ 011} and –p faces { 01 } exposed. The height of the crystal is 5-30 m and radius-height ratio is2:1. Mn atom concentration of 2. 6% (x=0.026) was determined using X-ray energy dispersive spectroscopy ( EDS). The crystals show low-temperature ferromagnetism with Curie temperature of 50K.