Abstract
Polyamide 5,6 (PA56) fibers were successfully prepared by melt-spinning technique. PA56 fibers were subjected to hot drawing process at different draw ratio and temperature. The effect of the drawing conditions on their mechanical properties such as tenacity, tensile modulus and breaking elongation were investigated by means of tensile test measurements. The results revealed that the tenacity and tensile modulus were found to be increased, while the elongation at break decreased with the draw ratio. The improvements of the mechanical properties could be attributed to the enhanced of the molecular orientation along the fiber axis and an increase in crystallinity. On the other hand, the PA56 fibers mechanical properties do not show significant difference with the drawing temperatures.
Publisher
Trans Tech Publications, Ltd.
Reference14 articles.
1. W.H. Carothers, J.W. Hill, STUDIES OF POLYMERIZATION AND RING FORMATION. XV. ARTIFICIAL FIBERS FROM SYNTHETIC LINEAR CONDENSATION SUPERPOLYMERS, J. Am. Chem. Soc. 54 (1932) 1579-1587.
2. M.I. Kohan, Nylon Plastics Handbook. Vol. 378. 1995: Hanser Publishers Munich, Germany.
3. P.W. Morgan, Condensation Polymers, Interscience Publishers New York, (1965).
4. E.K. Bolton, Chemical Industry Medal. Development of Nylon, Ind. Eng. Chem. 34 (1942) 53-58.
5. V.G. Bankar, J.E. Spruiell, J.L. White, Melt spinning of nylon 6: Structure development and mechanical properties of as-spun filaments, J. Appl. Polym. Sci. 21 (1977) 2341-2358.
Cited by
7 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献