Chromite and laterite ores from local sources were smelted in a vertical tube furnace with activated carbon as reducing agent at 1400°C to 1550°C using graphite crucible under argon atmosphere. It is shown that the grade and composition of the ore are the main factors determining the feasibility of smelting a mixture of chromite and laterite ores to produce a Fe-Ni-Cr crude alloy. The high recovery of iron and nickel in the alloy indicates the highly reducing condition prevailing in the smelting reduction experiments. It is also shown that the solubility of Ni in the slag increases with Ni concentration in the alloy and the FeO concentration in the slag. The chromium content of the slag increases with increasing iron content of the slag.
Publisher
Trans Tech Publications, Ltd.
Reference7 articles.
1. Kawahara, M., Toguri, J. and Bergman, R. (1988): Reducibility of Laterite Ores, Metallurgical and Materials Transactions B; 19B, 4; p.181.
2. Utigard, T. (1994): An Analysis of Slag Stratification in Nickel Laterite Smelting Furnaces Due to Composition and Temperature Gradients, Metallurgical and Materials Transactions B; 25B, 8; p.491.
3. Takano, C., Ferdinando, L., Cavallante, D., Martins, S. (2005): Recovery of Cr, Ni and Fe from dust generated in stainless, Mineral Processing and Extractive Metallurgy, Vol. 114, 201.
4. Uslu, E. and Eric, R., (1991): The reduction of chromite in liquid iron-chromium-carbon alloys, J. S. Afr. Inst. Min. Metal/. vol. 91, no. 11. 397-409.
5. Guangqiang, L. and Fumitaka, T. (2001); Distribution Equilibria of Fe, Co and Ni between MgO-saturated FeOx–MgO–SiO2 Slag and Ni Alloy, ISIJ International, Vol. 41, No. 11, p.1303–1308.
Cited by
6 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献