This paper discusses the issues regarding reliability of large-area (up to 25mm2) gate oxide on the C-face of 4H-SiC. We have shown that the TDDB characteristics of large-area gate oxide improved by separating gate oxidation processes into oxide growth by dry-oxidation and successive interface control by anneal in N2O ambient or that by wet-oxidation followed by anneal in H2 ambient. In particular, dry-oxidation followed by anneal in N2O ambient for interface treatment (dry+N2O process) is effective for the suppression of the random failure in TDDB characteristics. The estimated lifetime of gate oxide of less than 9mm2 by the dry+N2O process is six-digits larger than 30 years. In the case of the TDDB characteristics of 25mm2 gate oxide grown by the dry+N2O process, the initial and random failure in TDDB characteristics is dominant. However, even in this case, we have confirmed that the evaluated lifetime of 25mm2 gate oxide is more than 30 years. In order to clarify the mechanism of the degradation of the TDDB characteristics of large-area gate oxide, we examined the effect of the surface defect on the TDDB characteristics by observing the surface of each broken MOS capacitor after the TDDB test. We have found following results. (1) The initial failures in TDDB characteristics are mainly due to surface defects such as “down fall”, “comet”, and “triangular defect”. (2) The footprints of random failure do not correspond to the positions of smaller surface defects such as “bump”. Finally, we have found that the quality of the epitaxial layer affects random failure rate in the TDDB characteristics of large area gate oxide; the random failure in the TDDB characteristics of 25mm2 gate oxide on epitaxial layer grown by a certain epitaxial vendor is almost suppressed. However, the cause of the difference in TDDB characteristics is not identified.

Publisher

Trans Tech Publications, Ltd.

Subject

Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science

Cited by 17 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3