Dense Y3+-dopted α-SiAlON/BN composition ceramics was fabricated by hot pressing at 1900 °C for 60 min, and flextural strength at room and 1000 °C was investigated through three-point bending test. The results show that h-BN contribute to the densification of powder body, but h-BN have little affect on the key temperature region of sintering densification of α-SiAlON ceramics. When content of BN is lower, which didn’t affect on the phase transformation of α-SiAlON, but when content of BN is higher, besides of major phase α-SiAlON, a little of β-SiAlON was also formed. For the α-SiAlON/BN composite ceramics content of 20 wt.% h-BN, the higer flexural strength( room-temperature and 1000 °C) were abtained, the formation of β-SiAlON should be an important resonon for the higher strentgh, more important is , whose flexural strength at 1000 °C is higher 50 MPa than at room temperature, the differnce of thermal properties between SiAlON and BN should contribute to the improve of high-temperature flextural strength.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献