In this study, a commercial IrO2/TiO2 catalyst (75 wt% Ir, named “Benchmark”) for the oxygen evolution reaction (OER) is compared to a newly developed IrO(OH)x/TiO2 catalyst (45 wt% Ir, named “P2X”). Due to its lower Ir packing density and higher OER activity vs the Benchmark catalyst (440 vs 12 A gIr
−1 at 1.43 ViR-free), the P2X catalyst shows an improved PEM (proton exchange membrane) water electrolyzer performance at ≈9 times reduced Ir loading, however, only if a platinum-coated porous transport layer (PTL) at the anode is used. While the performance of membrane electrode assemblies (MEAs) with the Benchmark catalyst is unaffected when using an untreated titanium PTL, MEAs with the P2X catalyst perform poorly, which can be attributed to a contact resistance at the anode/PTL interface due to the low electrical conductivity of the P2X catalyst (0.7 S cm−1) vs the Benchmark catalyst (416 S cm−1) and the passivation of the Ti-PTL. A heat treatment procedure is used to transform the amorphous IrO(OH)x of the P2X catalyst into crystalline IrOx and, hence, increases its electrical conductivity. The optimum temperature for heat treatment to maximize electrical conductivity, OER activity and MEA performance will be evaluated.
Funder
German Federal Ministry of Education and Research
Publisher
The Electrochemical Society
Subject
Materials Chemistry,Electrochemistry,Surfaces, Coatings and Films,Condensed Matter Physics,Renewable Energy, Sustainability and the Environment,Electronic, Optical and Magnetic Materials
Cited by
66 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献