AbstractComplete recycling of Nd2Fe14B sludge by chemical methods has gained significance in recent years, however, it is not easy to recycle highly contaminant sludge and obtain product with good magnetic properties. Herein we report a simple four-step process to recycle the Nd2Fe14B sludge containing ~ 10% of contaminants. Sludge was leached in H2SO4 and selectively co-precipitated in two steps. In the first co-precipitation, Al3+ and Cu2+ were removed at pH 6. Thereafter, in the second co-precipitation Fe2+ and RE3+ sulfates were converted to the Fe and RE hydroxides. By annealing at 800 °C RE and Fe hydroxides precipitates were converted to the oxides and residual carbon was oxidized to CO2. After the addition of boric acid, Fe and RE oxides were reduced and diffused to the (Nd-RE)2Fe14B by calciothermic reduction diffusion. Removal of CaO by washing with D.I. water in glove box reduced the oxygen content (~ 0.7%), improved crystallinity and enhanced the magnetic properties significantly. Coercivity increased more than three times (from 242.71 to 800.55 kA/m) and Mr value was also enhanced up to more than 20% (from 0.481 to 0.605 T). In this green process Na2SO4 and Ca(OH)2 were produced as by-product those are non-hazardous and were removed conveniently.
Funder
National Research Foundation of Korea
National Institute of Science and Technology Human
National Research Council of Science and Technology
Publisher
Springer Science and Business Media LLC
Cited by
8 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献