Author:
Kim Seung Min,Pint Cary L.,Amama Placidus B.,Hauge Robert H.,Maruyama Benji,Stach Eric A.
Abstract
Detailed understanding of growth termination in vertically aligned single-walled carbon nanotubes (SWNTs) made via supergrowth, or water-assisted growth, remains critical to achieving the ultralong SWNTs necessary for next-generation applications. We describe the irreversible catalyst morphology evolution that occurs during growth, and which limits the lifetime of surface supported catalysts. Growth termination is strongly dependent on growth temperature, but not sensitive to C2H2:H2O ratio. In addition to both planar Ostwald ripening of small (sub-5 nm) Fe catalyst particles and diffusion of metal atoms into the alumina support, other features that contribute to growth termination or deceleration are described, including center-of-mass particle motions and coalescence of smaller species of surface supported Fe nanoparticles. Additionally, a temperature-induced structural transition in the alumina catalyst support is found to be coincident with abrupt growth termination at temperatures of 800 °C and higher. In situ electron microscopy observations are used to directly support these observations.
Publisher
Springer Science and Business Media LLC
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Cited by
41 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献