Abstract
ABSTRACTResults are presented for a large number of aqueous leach tests on glass specimens doped with 237Np, 238Pu, 239pu, 241Am or 244Cm. The effects of the leaching mode (static or dynamic), temperature and environmental materials are discussed. The amount of actinides contained in the alteration film is characterized by the retention factor RF = NL(B)/NL(act). The neptunium retention factor ranged from 1 to 10 depending on the test conditions; for plutonium and americium, the retention factor varied from 6 to 1300.In general, the retention factor increased with the temperature. The very important influence of the environmental materials shows that there is competition for actinide retention between the alteration film and the surrounding materials, but in every case the amount of ca activity released into solution is very low.
Publisher
Springer Science and Business Media LLC
Reference12 articles.
1. R7T7 Nuclear Waste Glass Behavior in Moist Clay: Role of the Clay Mass/Glass Surface Area Ratio
2. 11. Dussossoy J.L. , Chouchan J.L. , Bouchon M. and Vernaz E. , Leaching Sensitivity to Geologic Environmental Parameters, CCE contract No FI 1W 0027, Final Report, EUR 13603 EN.
3. Key Parameters of Glass Dissolution in Integrated Systems
4. Effect of Environmental Materials on Aqueous Corrosion of R717 Glass;Godon;Scientific Basis for Nuclear Waste Management XII, Mat. Res. Soc. Symp. Proc.,1989
Cited by
25 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献