Author:
Blank V.,Popov M.,Lvova N.,Gogolinsky K.,Reshetov V.
Abstract
The new procedure for the hardness measurements of superhard materials including diamond using the scanning force microscope with the ultrahard fullerite C60 tip was developed. It is shown that diamond is plastically deformed under the indentation by the ultrahard fullerite indenter at room temperature. Now the correct measurements of diamond hardness have become possible. The hardness values measured are 137 ± 6 and 167 ± 5 GPa for the diamond faces (100) and (111), respectively.
Publisher
Springer Science and Business Media LLC
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Reference19 articles.
1. 16. Lyssenko V. , Astashenkov A. , Gogolinsky K. , and Reshetov V. , Proc. 7th Int. Conf. Metrology and Properties of Engineering Surfaces (Göteborg, Sweden, 1997) (in press).
2. Interpretation of force curves in force microscopy
Cited by
54 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献