Influence of Temperature from 20 to 100 °C on Specific Surface Energy and Fracture Toughness of Silicon Wafers

Author:

Lapitskaya V. A.1,Kuznetsova T. A.1,Chizhik S. A.1

Affiliation:

1. A.V. Luikov Heat and Mass Transfer Institute of NAS of Belarus; Belarusian National Technical University

Abstract

The influence of temperature in the range from 20 to 100 °C on the specific surface energy and fracture toughness of standard silicon wafers of three orientations (100), (110) and (111) was studied. Silicon wafers were heated on a special thermal platform with an autonomous heating controller, which was installed under the samples. At each temperature, the samples were kept for 10 min. The specific surface energy γ after exposure to temperature was determined by atomic force microscopy (AFM). Fracture toughness during and after exposure to temperature was determined by indentation followed by visualization of the deformation region using AFM. It has been established that the specific surface energy γ of Si wafers with orientation (100) and (111) increases with increasing temperature from 20 to 100 °C, and for orientation (110) it increases at temperatures from 20 to 80 °C, and then decreases. The diagonal length d of indentation marks, performed both during the heating process and after heating, decreases by increasing the temperature from 20 to 100 °C. The crack length c decreases on silicon wafers during indentation during heating from 20 to 100 °C, and after exposure to temperature, the length increases. When the plates are exposed to temperature, the fracture toughness KIC increases with increasing temperature: for orientation (100) – up to 1.61 ± 0.08 MPa·m1/2, for (110) – up to 1.60 ± 0.08 MPa·m1/2 and for (111) – up to 1.66 ± 0.04 MPa·m1/2. A direct correlation was established between KIC, measured during  exposure to temperature, and an inverse correlation between KIC measured after exposure to temperature and specific surface energy for the (100) and (111) orientations. An inverse correlation was obtained by KIC at the (110) orientation when exposed to temperatures of 20–40 and 80–100 °C, and after exposure, a direct correlation was obtained. At 60 °C there is no correlation. The results obtained can be used to improve the mechanical properties of silicon wafers used in solar cells and microelectromechanical systems (operating at temperatures up to 100 °C).

Publisher

Belarusian National Technical University

Subject

General Earth and Planetary Sciences,Water Science and Technology,Geography, Planning and Development

Reference17 articles.

1. Tilli M, Paulasto-Kröckel M, Petzold M, Theuss H, Motooka T, Lindroos V. Handbook of Silicon Based MEMS Materials and Technologies. Elsevier, 2020.636 p.

2. Masolin A, Bouchard PO, Martini R, Bernacki M. Thermo-mechanical and fracture properties in singlecrystal silicon, Journal of Materials Science. 2013;48: 979-988. DOI: 10.1007/s10853-012-6713-7

3. Hashimov AM, Hasanli ShM. Influence the heat treatment on the mechanical characteristics of silicon plates, Fizika. 2004;CILD X №4:71-73.

4. Courtney TH. Mechanical Behavior of Materials: Second Edition. Waveland Press;2005. 733 p.

5. Lauener CM, Petho L, Chen M, Xiao Y, Michler J, Wheeler JM. Fracture of Silicon: Influence of rate, positioning accuracy, FIB machining, and elevated temperatures on toughness measured by pillar indentation splitting. Materials & Design. 2018;142:340-349. DOI: 10.1016/j.matdes.2018.01.015

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3