Abstract
In this work, aluminum alloy 7075-T651 was welded by using customized Al-Cu-Si and Al-Cu-Mg-Zn filler wire during gas tungsten arc welding. The liquation cracking susceptibility of the joints was tested under a circular-patch welding experiment. Besides, the temperature vs. solid fraction curves (T-fS) was calculated for different samples to reveal the formation mechanism of liquation cracking. The joint was susceptible to liquation cracking if (fS)weld > (fS)workpiece during the cooling stage. The results of the circular-patch welding experiment show that the liquation cracking susceptibility of the joint by using ER5356, Al-Cu1.5-Si4.5, Al-Cu3.0-Si2.5, Al-Cu4.5-Si1.5, Al-Cu2.3-Mg2.3-Zn6.6 and Al-Cu2.2-Mg2.0-Zn7.8 filler metal is 22.8%, 8.3%, 2.8%, 2.8%, 3.3% and 1.4%, respectively. The mechanical test shows that the data dispersion of the 7075 gas tungsten arc welding joint can be decreased by eliminating the liquation crack.
Funder
National Natural Science Foundation of China
Beijing Municipal Natural Science Foundation
the 38th China-Poland intergovernmental Joint S&T Committee Meeting, Personal Exchange Project
Subject
General Materials Science
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献