Innovative Approach for the Evaluation of the Mechanical Behavior of Dissimilar Welded Joints

Author:

Carone SimoneORCID,Corigliano PasqualinoORCID,Epasto GabriellaORCID,Moramarco VincenzoORCID,Palomba GiuliaORCID,Pappalettera Giovanni,Casavola Caterina

Abstract

This study aims to propose a thorough experimental methodology to assess the mechanical quality of dissimilar joints. This comprehensive approach investigates the fatigue behavior by exploiting the thermographic method, accompanying and correlating the results with information obtained from extensive measurements of residual stresses and detailed evaluation of fracture surfaces. The integration of the information obtained by this hybrid approach allows for a deeper understanding in terms of fatigue behavior even in complicated situations as those represented by dissimilar welded joints. A complex laser-welded Ti6Al4V/Inconel 625 dissimilar joint, obtained using intermediate inserts of Vanadium and AISI 304, was considered as case study. The residual stresses, both longitudinal and transverse to the weld beads, were measured on surface by means of X-ray diffraction, whereas, for in-depth measurements, the multiple-cut contour method was implemented to determine full 2D maps of longitudinal residual stresses with the first cut, and transverse stresses in the Vanadium insert with the second cut. In the investigation of longitudinal residual stresses, the area mostly affected by harmful tensile residual stresses is the weld between the stainless steel and Vanadium, where the maximum value of about 560 MPa is reached; the analysis of transverse residual stresses highlighted a maximum value of 350 MPa at the core of the Vanadium insert. The fatigue behavior of the joints was investigated along with a detailed analysis of the fractured surfaces by scanning electron and confocal microscopes. The analysis of the fracture surfaces indicated that the failure modes are mainly related to the occurrence of defects on the crack path, especially at stress range higher than 200 MPa, for which a large number of pores cluster were detected. Nevertheless, the crack initiation is usually on the side of Vanadium. When the crack path deviates on the stainless-steel region, the fracture mode is brittle due to high residual stresses.

Funder

Italian Ministry of Education, University and Research

Publisher

MDPI AG

Subject

General Materials Science,Metals and Alloys

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3