Affiliation:
1. Xi’an Modern Control Technology Research Institute, Xi’an 710065, China
2. School of Materials Science & Engineering, Chang’an University, Xi’an 710061, China
Abstract
In this work, Al2O3 nanoceramics were prepared by spark plasma sintering of amorphous powders and polycrystalline powders with similar particle sizes. Effective comparisons of sintering processes and ultimate products depending on starting powder conditions were explored. To ensure near-full density higher than 98% of the Al2O3 nanoceramics, the threshold temperature in SPS is 1450 °C for polycrystalline Al2O3 powders and 1300 °C for amorphous powders. The low SPS temperature for amorphous powders is attributed to the metastable state with high free energy of amorphous powders. The Al2O3 nanoceramics prepared by amorphous powders display a mean grain size of 170 nm, and superior mechanical properties, including high bending strength of 870 MPa, Vickers hardness of 20.5 GPa and fracture toughness of 4.3 MPa∙m1/2. Furthermore, the Al2O3 nanoceramics prepared by amorphous powders showed a larger dynamic strength and dynamic strain. The toughening mechanism with predominant transgranular fracture is explained based on the separation of quasi-boundaries.
Funder
National Nature Science Foundation of China
Fundamental Research Funds for the Central Universities, CHD
Subject
General Materials Science
Cited by
4 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献