Abstract
The hot tensile deformation and fracture mechanisms of a Ti-5Al-5Mo-5V-1Cr-1Fe alloy with bimodal and lamellar microstructures were investigated by in situ tensile tests under scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD). The results show that the main slip deformation modes are prismatic slip ({11¯00}<112¯0>) and pyramidal slip ({11¯01}<112¯0>) under tension at 350 °C. In the bimodal microstructure, several parallel slip bands (SBs) first form within the primary α (αP) phase. As the strain increases, the number of SBs in the αP phase increases significantly and multislip systems are activated to help further coordinate the increasing deformation. Consequently, the microcracks nucleate and generally propagate along the SBs in the αP phase. The direction of propagation of the cracks deflects significantly when it crosses the αP/β interface, resulting in a tortuous crack path. In the lamellar microstructure, many dislocations pile up at the coarse-lath α (αL) phase near the grain boundaries (GBs) due to the strong fencing effect thereof. As a result, SBs develop first; then, microcracks nucleate at the αL phase boundary. During propagation, the cracks tend to propagate along the GB and thus lead to the intergranular fracture of the lamellar microstructure.
Funder
the State Key Laboratory of Powder Metallurgy
Subject
Inorganic Chemistry,Condensed Matter Physics,General Materials Science,General Chemical Engineering
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献