Author:
Li Xin,Niu Shuxin,Wang Dongsheng,Li Jie,Jiao Qi,Guo Xinlong,Xu Xiqing
Abstract
Silica-based ceramic cores play key roles in the casting of aeroengine blades, but they are highly limited by the poor high-temperature mechanical property. Here, fused mullite (FM) and sintered mullite (SM) powders were modified in silica-based ceramic cores, and the microstructure evolution and crystallization kinetics of ceramic cores depending on mullite types were studied. The ceramic cores with FM showed a dense microstructure and superior mechanical properties compared to those with SM. The ceramic cores with 10 wt.% of FM showed a crystallization activation energy of 1119.5 kJ/mol and a crystallization exponent of 1.74, and the values of 938.4 kJ/mol and 1.86 as SM were employed; the decreased crystallization activation energy and the elevated crystallization exponent by SM suggested that the excess impurities of alkali oxides and alkaline-earth oxides significantly promoted the crystallization of cristobalite. Even though the ceramic cores with mullite powders decreased slightly in the room-temperature mechanical property, their high-temperature flexure strength and creep deformation resistance were enhanced. The ceramic cores with 10 wt.% of FM showed excellent comprehensive performance, with linear shrinkage of 0.69%, room-temperature strength of 18.9 MPa, and high-temperature strength of 15.5 MPa, which satisfied the demands for hollow-blade casting.
Funder
National Nature Science Foundation of China
Fundamental Research Funds for the Central Universities
Subject
General Materials Science
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献