Abstract
Through studying the effects of the Al–5Ti-x(Mg–30%Ce) refiner on the microstructure of the Al–7Si alloy, we investigated the hardness, tensile, and impact properties of the Al–Si alloy before and after refinement. The refinement results show that Mg–30%Ce can improve the refinement effect of Al–5Ti on Al–7Si, and also refine α-Al and eutectic Si in Al–7Si. When 2%Mg–30%Ce is added, the refining effect of the aluminum–silicon alloy is most obvious. After refinement, the hardness and tensile properties of the Al–7Si alloy improve. When 2%Mg–30%Ce is added to the refiner, the tensile properties of the Al–Si alloy are the best. Dynamic mechanical tests were conducted on refined Al–7Si alloy. The impact toughness of Al–7Si–(Al–5Ti-2(Mg–30%Ce) improved and the impact toughness reached 34.91 J/cm2, which is 78.7% higher than that of Al–7Si–(Al–5Ti) specimens. The separate Hopkinson pressure bar test results show that, under a high strain rate, the strain rate sensitivity of the prepared Al–Si alloy is significant. The specimens of Al–7Si–(Al–5Ti-2(Mg–30%Ce) demonstrated the best anti-impact performance at the same velocity.
Subject
General Materials Science,Metals and Alloys
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献