Stainless-steel slag was used to prepare glass-ceramics, which could solidify
chromium (Cr) in the slag. The migration and distribution state of chromium
in the slag during the preparation of the glass-ceramics have a great
influence on the chromium fixation ability of the glass-ceramics. In this
paper, the effects of Al2O3 content in the glass-ceramics on the migration
and distribution of chromium during the nucleation and crystallization
steps, and on the chromium fixation effect of the glass-ceramics were
systematically studied. The results show that in the nucleation stage, with
the increase of Al2O3 content, the number of chromium spinel (Cr-spinel)
nanocrystals formed in the glass first increases and then decreases, and Cr
in the glass phase gradually migrates to Cr-spinel nanocrystals. TEM and XPS
analyses show that during crystallization, part of Cr in Cr-spinel diffuses
into diopside lattice, and the other part of Cr still exists in Cr-spinel
wrapped by diopside. Cr in the glass phase also diffuses and migrates into
the diopside lattice with the formation of diopside crystals. The optimal
Al2O3 content is 11.8wt.%, which results in 97.94wt.% of the total Cr being
fixed in the diopside crystalline phase. The ability of chromium fixation is
very high giving a very low Cr leaching concentration of 0.004mg/l. The
research results provide theoretical and technical support for increased
chromium fixation and realizing harmless and high-value utilization of
stainless-steel slag.