In Situ Surface Biodegradation of Restorative Materials

Author:

Padovani GC1,Fúcio SBP2,Ambrosano GMB3,Sinhoreti MAC4,Puppin-Rontani RM

Affiliation:

1. Gislaine C Padovani, DDS, MS, PhD, Dental Materials, Piracicaba Dental School, Piracicaba, SP, Brazil

2. Suzana Beatriz P Fúcio, DDS, MS, PhD, Pediatric Dentistry, Herminio Ometto foundation, Uniararas University, Araras, SP, Brazil

3. Gláucia Maria Bovi Ambrosano, DDS, MS, PhD, Community Dentistry Department, State University of Campinas, Piracicaba, SP, Brazil

4. Mário Alexandre Coelho Sinhoreti, DDS, MS, PhD, Restorative Dentistry, Piracicaba Dental School, University of Campinas, Piracicaba, SP, Brazil

Abstract

SUMMARY This study aimed to evaluate the surface characteristics of restorative materials (roughness, hardness, chemical changes by energy-dispersive spectroscopy [EDX], and scanning electron microscopy [SEM]) submitted to in situ biodegradation. Fifteen discs of each material (IPS e.max [EM], Filtek Supreme [FS], Vitremer [VI], Ketac Molar Easymix [KM], and Amalgam GS-80 [AM]) were fabricated in a metallic mold (4.0 mm × 1.5 mm). Roughness, hardness, SEM, and EDX were then evaluated. Fifteen healthy volunteers used a palatal device containing one disc of each restorative material for seven days. After the biodegradation, the roughness, hardness, SEM, and EDX were once again evaluated. Data obtained from the roughness and hardness evaluations were submitted to Kolmogorov-Smirnov and Tukey-Kramer tests (p<0.05). All esthetic restorative materials showed a significant increase in the roughness after biodegradation. Before biodegradation, significant differences in the hardness among the materials were seen: EM>AM>FS>KM>VI. After biodegradation, the hardness was significantly altered among the materials studied: EM>AM>FS=KM>VI, along with a significant increase in the hardness for AM, KM, and VI. SEM images indicated degradation on the surface of all materials, showing porosities, cracks, and roughness. Furthermore, after biodegradation, FS showed the presence of Cl, K, and Ca on the surface, while F was not present on the VI and KM surfaces. EM and AM did not have alterations in their chemical composition after biodegradation. It was concluded that the dental biofilm accumulation in situ on different restorative materials is a material-dependent parameter. Overall, all materials changed after biodegradation: esthetic restorative materials showed increased roughness, confirmed by SEM, and the ionomer materials and silver amalgam showed a significantly higher hardness. Finally, the initial chemical composition of the composite resin and ionomer materials evaluated was significantly altered by the action of the biofilm in situ.

Publisher

Operative Dentistry

Subject

General Dentistry

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3