Abstract
Abstract
We report on fabrication and characterization of layered, tungsten doped, spherical about 2 mm diameter microcrystalline diamond ablator shells for inertial confinement fusion (ICF) experiments at the National Ignition Facility. As previously reported, diamond ICF ablator shells can be fabricated by chemical vapor deposition (CVD) on solid spherical silicon mandrels using an ellipsoidal microwave plasma reactor. In the present work, we further developed these ablator shells by embedding a W-doped diamond layer sandwiched between two undoped diamond regions. W incorporation in diamond was achieved by adding tungsten hexacarbonyl to the CH4/H2 CVD feed gas. We observe that the W doping concentration decreases with increasing deposition rate which, in turn, is controlled by adjusting the total gas pressure. Cross sectional microstructural analysis reveals sharp interfaces between doped and undoped regions of the diamond shell and uniform W distribution with concentrations up to about 0.3 at.%. At higher W concentrations (>0.3 at.%) formation of tungsten carbide precipitates is observed. Using a 3‐shock 1.6 MJ laser pulse, the targets described in this work produced the first laser driven implosion to break the 1 × 1016 neutron yield barrier, followed by experiments (described in future publications) with similar targets and slightly more laser energy producing yields as high as 4 × 1017.
Subject
Condensed Matter Physics,Nuclear and High Energy Physics
Cited by
10 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献