Abstract
Abstract
In the present study, a Co-rich CoCrNi-AlTi high-entropy alloy was designed and fabricated by hot forging and 700 °C for 8 h annealing process. The microstructure of the resultant alloy was composed of three multicomponent-phases with the face-centered cubic (FCC) structure, hexagonal close-packed (HCP) structure and L12 structure, respectively. The alloy exhibited a remarkable combination of tensile yield strength (gigapascal scale) and plasticity (uniform strain over 30%) at both room and cryogenic temperatures. The cooperative operation of multiple mechanisms consisting of refined-grain strengthening, second-phase strengthening, precipitation strengthening, stacking faults and phase-transformation toughening was suggested to be responsible for the excellent mechanical response.
Funder
National Natural Science Foundation of China
Subject
Metals and Alloys,Polymers and Plastics,Surfaces, Coatings and Films,Biomaterials,Electronic, Optical and Magnetic Materials
Cited by
19 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献