Author:
Sun Bingxin,Chuai Chengzhi,Luo Si,Guo Ying,Han Chunyang
Abstract
Abstract
Poly(butylene succinate) (PBS) with different ratios of modified talc was prepared by twin-screw extruding. The effect of different loading amounts of talc on the mechanical, thermal, and crystallization properties of PBS was investigated. The mechanical test results indicate that the stiffness of the composites was increased linearly with increasing talc content, and the tensile strength and elongation stayed at relatively high levels when the talc amount is <15 phr. Thermal gravimetric analysis showed that the thermal stability of PBS composites was improved notably with a small amount (5–10 phr) of talc; however, high loading of talc did not help further improve the thermal stability. Differential scanning calorimetry data showed that the melting enthalpy (ΔHm), crystallization enthalpy (ΔHc), and crystallinity degree (Xc) decreased when the talc increased and crystallization temperature (Tc) was moving to relatively high values. The results of X-ray diffraction demonstrated that the incorporation of talc inhibited the PBS crystallization behavior significantly but did not change the crystal structure. Scanning electron microscopic studies indicated that the homogeneous dispersion and smoother fracture surfaces of the composite became inhomogeneous and coarse with higher talc loading.
Subject
Materials Chemistry,Polymers and Plastics,General Chemical Engineering
Reference76 articles.
1. ST MS;Lim;Chem Mater,2002
2. Karger;García Gutiérrez;Chem Phys Lett,2004
3. Karger;García Gutiérrez;Chem Phys Lett,2004
4. Thermal stability of poly(l-lactide)/poly(butylene succinate)/clay nanocomposites
Cited by
16 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献