Phase composition of polycrystalline HfNx (0.45 ≤ x ≤ 1.60) and effects of low-energy ion irradiation on microstructure, texture, and physical properties

Author:

Seo Hwan-Seok1ORCID,Lee Taeyoon2ORCID,Kim Hyungjun2ORCID,Petrov Ivan3ORCID,Greene J. E.3

Affiliation:

1. Department of Materials Science and Engineering, Yonsei University 1 , 50 Yonsei-ro, Seodaemun-gu, Seoul 03722, Republic of Korea

2. School of Electrical and Electronic Engineering, Yonsei University 2 , 50 Yonsei-ro, Seodaemun-gu, Seoul 03722, Republic of Korea

3. Materials Research Laboratory and Materials Science Department, University of Illinois 3 , 104 South Goodwin, Urbana, Illinois 61801

Abstract

We have investigated the phase composition of HfNx as a function of x and the effects of low-energy ion irradiation on the microstructure and physical properties of polycrystalline layers grown on SiO2 at 350 °C by ultrahigh vacuum reactive dc magnetron sputtering of Hf in mixed N2/Ar discharges. X-ray diffraction and Rutherford backscattering spectrometry results show that the phases obtained in polycrystalline HfNx layers with increasing x are hcp-structure α-Hf:N (x ≲ 0.6); multiphase mixtures consisting of α-Hf, NaCl-structure δ-HfN, rhombohedral ɛ-Hf3N2, and/or ζ-Hf4N3 (0.6 ≲ x ≲ 0.9); δ-HfN single phase (0.9 ≲ x ≲ 1.3); and mixtures of δ-HfN and higher nitrides (x ≳ 1.3). HfNx layers with 0.9 ≲ x ≲ 1.2 grown under mild ion irradiation (incident ion energy Ei ≃ 7 eV and ion-to-Hf flux ratios Ji/JHf = 1−3) are underdense with mixed orientation, low in-plane stress, and rough surface morphology due to limited adatom mobilities resulting in kinetic roughening and atomic shadowing during film growth. However, the use of intense ion irradiation (Ei = 25 eV and Ji/JHf = 4−20) results in HfNx layers, which are fully dense with strongly 111-oriented texture, compressive in-plane stress, and smooth surfaces due to ion irradiation enhanced adatom surface mobilities. In addition, the latter films have lower resistivity and higher hardness. For stoichiometric δ-HfN layers, ρ decreases from 69.7 to 35.2 μΩ cm and H increases from 22.1 to 27.4 GPa, with increasing ion-irradiation intensity. However, for HfNx layers with 1.2 ≲ x ≲ 1.6, the correspondingly higher steady state atomic N surface coverages during deposition alter growth kinetics in favor of 001 texture with a fully dense structure and compressive in-plane stress.

Funder

U.S. Department of Energy

Korea Medical Device Development Fund

National Research Foundation of Korea

Publisher

American Vacuum Society

Subject

Surfaces, Coatings and Films,Surfaces and Interfaces,Condensed Matter Physics

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3