Dissimilar Metal Weld Pipe Fracture Testing: Analysis of Results and Their Implications

Author:

Rudland D.1,Lukes R.1,Scott P.2,Olson R.2,Cox A.2,Shim D.-J.3

Affiliation:

1. US Nuclear Regulatory Commission, Washington, DC

2. Battelle, Columbus, OH

3. Engineering Mechanics Corporation of Columbus, Columbus, OH

Abstract

Typically in flaw evaluation procedures, idealized crack shapes are assumed for both subcritical and critical crack analyses. Past NRC-sponsored research have developed estimation schemes for predicting the load-carrying capacity of idealized cracks in nuclear grade piping and similar metal welds at the operating conditions of nuclear power reactors. However, recent analyses have shown that growth of primary water stress corrosion cracks (PWSCC) in dissimilar metal (DM) welds is not ideal; in fact, very unusual complex crack shapes may form, i.e., a very long surface crack that has a finite length through-wall crack in the same plane. Even though some experimental data on base metals exists to demonstrate that complex shaped cracks in high toughness materials fail under limit load conditions, other experiments demonstrate that the tearing resistance is significantly reduced. At this point, no experimental data exists for complex cracks in DM welds. In addition, it is unclear whether the idealized estimation schemes developed can be used to predict the load-carrying capacity of these complex-shaped cracks, even though they have been used in past analyses by the nuclear industry. Finally, it is unclear what material strength data should be used to assess the stability of a crack in a DM weld. The NRC Office of Nuclear Regulatory Research, with their contractor Battelle Memorial Institute, has concluded an experimental program to confirm the stability behavior of complex shaped circumferential cracks in DM welds. A combination of full-scale pipe experiments and a variety of laboratory experiments were conducted. A description of the pipe test experimental results is given in a companion paper. This paper describes the ongoing analyses of those results, and the prediction of the load-carrying capacity of the circumferential cracked pipe using a variety of J-estimation scheme procedures. Discussions include the effects of constraint, appropriate base metal material properties, effects of crack location relative to the dissimilar base metals, and the limitations of the currently available J-estimation scheme procedures. This paper concludes with plans for further development of J-estimation scheme procedures for circumferential complex cracks in DM welds.

Publisher

American Society of Mechanical Engineers

Cited by 3 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3