Blunt Crack Initiation and its Transition to Sharp Cracks in Pipeline Steel in Near-Neutral pH Solution

Author:

Fang B.12,Eadie R. L.3,Elboujdaini M.4

Affiliation:

1. RAE Engineering and Inspection Ltd., Calgary, AB, Canada

2. Chinese Academy of Sciences, Shenyang, China

3. University of Alberta, Edmonton, AB, Canada

4. CANMET Materials Technology Laboratory, Ottawa, ON, Canada

Abstract

This paper reviews our research into pipeline stress corrosion cracking (SCC) in near-neutral pH (NNpH) environment to help understand the mechanisms on pit-to-crack transition and early growth to contribute to pipeline integrity management so that the risk of failure can be avoid or reduced. Pitted specimens by using two different techniques (passivation/immersion and electrochemical methods) were cyclically loaded in NNpH environment sparged with 5% CO2 / balance N2 gas mixture at high stress ratios (minimum stress/maximum stress), low strain rates and low frequencies which are close to the operational pipelines in the field. Blunt cracks initiation was seen first and associated with the pit geometry, and most of the blunt cracks were observed to have initiated from the corrosion pits that had the pit depth to surface width aspect ratios greater than 0.5. The blunt crack growth was engendered by anodic dissolution, which was facilitated by stress. So it was called as stress facilitated dissolution crack growth. These blunt cracks had considerably large crack tip width to crack mouth width aspect ratios, and the majority were below 0.5 to 0.6 mm deep, and considered dormant. Once cracks surpassed the critical value, around 0.5 to 0.6 mm, the cracks would be reactivated and the crack tip width to crack mouth width ratios became significantly smaller. Meanwhile, more hydrogen would be trapped in the plastic zones. Thus, hydrogen would play an important role in the crack propagation. So in this stage, cracks tended to become sharp and the mechanism was referred to hydrogen facilitated cracking. The observations from the field can be interpreted very well by using the proposed models. It was proposed that two different mechanisms are responsible for the early-stage crack growth and sharp cracks be removed to reduce the risk of failure in pipelines.

Publisher

American Society of Mechanical Engineers

Cited by 1 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3