Improved connective integration of a degradable 3D-nano-apatite/agarose scaffold subcutaneously implanted in a rat model

Author:

García-Honduvilla Natalio123,Coca Alejandro1,Ortega Miguel A12,Trejo Cynthia4,Román Jesús5,Peña Juan5,Cabañas M Victoria5,Vallet Regi Maria25,Buján Julia12

Affiliation:

1. Departments of Medicine and Medical Specialties, Faculty of Medicine and Health Sciences, University of Alcalá. Alcalá de Henares, Madrid, Spain. Ramón y Cajal Institute of Sanitary Research (IRYCIS), Madrid, Spain

2. Networking Biomedical Research Center on Bioengineering, Biomaterials and Nanomedicine (CIBER-BBN), Madrid, Spain

3. Defense University Center of Military Central Academy (CUD-ACD), Madrid, Spain

4. Research Group on Stem Cells and Tissue Engineering (GICTIT), Laboratory of Research in Dentistry Almaraz, FES Iztacala, UNAM, Mexico

5. Department of Inorganic and Bioinorganic Chemistry, Faculty of Pharmacy, UCM, Institute of Health Research Hospital 12 de Octubre i + 12, 28040-Madrid, Spain

Abstract

In this work, we evaluate the tissue response and tolerance to a designed 3D porous scaffold composed of nanocrystalline carbonate-hydroxyapatite and agarose as a preliminary step in bone repair and regeneration. These scaffolds were subcutaneously implanted into rats, which were sacrificed at different times. CD4+, CD8+ and ED1+ cells were evaluated as measurements of inflammatory reaction and tolerance. We observed some inflammatory response early after subcutaneous implantation. The 3D interconnected porosity increased scaffold integration via the formation of granulation tissue and the generation of a fibrous capsule around the scaffold. The capsule is initially formed by collagen which progressively invades the scaffold, creating a network that supports the settlement of connective tissue and generating a compact structure. The timing of the appearance of CD4+ and CD8+ cell populations is in agreement with the resolved inflammatory response. The appearance of macrophage activity evidences a slow and gradual degradation activity. Degradation started with the agarose component of the scaffold, but the nano-apatite was kept intact for up to 30 days. Therefore, this apatite/agarose scaffold showed a high capacity for integration by a connective network that stabilizes the scaffold and results in slow nano-apatite degradation. The fundamental properties of the scaffold would provide mechanical support and facilitate bone mobilization, which is of great importance in the masticatory system or large bones.

Publisher

SAGE Publications

Subject

Biomedical Engineering,Biomaterials

Cited by 9 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3