Contact Damage Resistance and Strength Degradation of Glass-infiltrated Alumina and Spinel Ceramics

Author:

Jung Y.-G.1,Peterson I.M.1,Pajares A.1,Lawn B.R.1

Affiliation:

1. Materials Science and Engineering Laboratory, National Institute of Standards and Technology, Gaithersburg, Maryland 20899

Abstract

All-ceramic crowns are coming into widespread use because of their superior esthetics and chemical inertness. This study examines the hypothesis that glass-infiltrated alumina and spinel core ceramics are resistant to damage accumulation and strength degradation under representative oral contact conditions. Accordingly, Hertzian indentation testing with hard spheres is used to evaluate damage accumulation in alumina and spinel ceramics with different pre-form grain morphologies and porosities. Indentation stress-strain curves measured on fully infiltrated materials reveal a marked insensitivity to the starting pre-form state. The glass phase is shown to play a vital role in providing mechanical rigidity and strength to the ceramic structures. All the infiltrated ceramics show subsurface cone fracture and quasi-plastic deformation above critical loads Pc (cracking) and Py (yield), depending on sphere radius, with Py < Pc. Strength degradation from accumulation of damage in Hertzian contacts above these critical loads is conspicuously small, suggesting that the infiltrated materials should be highly damage-tolerant to the "blunt" contacts encountered during mastication. Failure in the strength tests originates from either cone cracks ("brittle mode") or yield zones ("quasi-plastic mode"), with the brittle mode more dominant in the spinels and the quasi-plastic mode more dominant in the aluminas. Multi-cycle contacts at lower loads, but still above loads typical of oral function, are found to be innocuous up to 105 cycles in air and water, although contacts at 106 cycles in water do cause significant strength degradation. By contrast, contacts with Vickers indenters produce substantial strength losses at low loads, suggesting that the mechanical integrity of these materials may be compromised by inadvertent "sharp" contacts.

Publisher

SAGE Publications

Subject

General Dentistry

Reference32 articles.

1. A Critical Evaluation of Indentation Techniques for Measuring Fracture Toughness: I, Direct Crack Measurements

2. Anusavice KJ (1989). Criteria for selection of restorative materials : properties vs technique sensitivity. In: Quality evaluations of dental restorations. Anusavice KJ, editor. Chicago: Quintessence, pp. 15-56.

3. Indentation fatigue

Cited by 44 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3