Abstract
The purpose of this work is to understand the impact of superheated water hydrolysis treatment on the chemical properties of wool, and compare it with a conventional method of alkaline hydrolysis. The effects of hydrolysis temperature and concentration of alkali on the properties of wool were investigated. Superheated water hydrolysis was carried out at the temperatures of 140℃ and 170℃, with a material to liquor ratio of 1:3 for 1 hour. In conventional alkaline hydrolysis, the experiments were carried out in the same conditions using potassium hydroxide (KOH) and calcium oxide (CaO) with a concentration in the range of 5%–15% on the fiber weight (o.w.f.). The effects of hydrolysis temperature and alkali concentrations on wool properties were checked using optical and scanning electron microscopy. It was observed that the hydrolyzates obtained in both cases contained low molecular weight proteins and amino acids. Both the hydrolysis processes resulted in degradation of the wool fibers. However, superheated steam hydrolysis is an environmentally friendly and less expensive process, as it is performed using water as a solvent. The wool hydrolyzates produced using superheated water hydrolysis could find a potential application in agriculture, such as fertilization, soil improvement and suchlike.
Subject
Polymers and Plastics,Chemical Engineering (miscellaneous)
Cited by
42 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献