Affiliation:
1. School of Civil and Transportation Engineering, Hebei University of Technology, Tianjin, China
2. Hebei Civil Engineering Technology Research Center, Hebei University of Technology, Tianjin, China
Abstract
The improved high-performance polymer cement mortar (PCM) and glass fiber reinforced plastic (GFRP) system reinforcement was used in the research to strengthen and repair the masonry structure, so as to improve its bond stress, anchoring force, and integral performance without changing the original structure and further study the shear performance of masonry structure strengthened by the combination of the two. The optimum ratio of improved high-performance PCM was determined by analyzing the bend-press ratio of PCM test block. Improved high-performance PCM and GFRP were combined to strengthen the damaged masonry wall, and a five-piece masonry wall composed of “improved high-performance PCM+ with or without GFRP+ different original wall failure modes before reinforcement” was designed. Through diagonal loading shear test, the shear strength, vertical displacement, horizontal relative displacement, and failure models of masonry walls were obtained, and the effects of five different reinforcement methods and different materials on shear strength, stiffness, ductility, and failure modes of masonry walls were studied. The results show that compared with the unreinforced original wall, the shear strength of the masonry wall reinforced with the improved O4PCM is 43.5% higher, and its stiffness is also greatly improved, but the failure mode is still brittle failure; the shear strength of masonry walls strengthened by O4PCM and GFRP is 6.5% higher than that of masonry walls strengthened by O4PCM alone, and the stiffness is also increased. Its failure mode changes from brittle failure to ductile failure; with a failure mode of ductile failure, the shear strength of masonry walls strengthened by P4PCM and GFRP and that strengthened by P6PCM and GFRP are 4.8% and 12.7% higher than that strengthened by O4PCM and GFRP, respectively, and the stiffness is also increased compared with that strengthened by O4PCM and GFRP. After experimental comparison, it is the best scheme to strengthen masonry wall with improved P6PCM and GFRP.
Funder
The Nature Fund Project of Hebei Province, China
Subject
Building and Construction,Civil and Structural Engineering
Reference28 articles.
1. ASTME519-02 (2001) Detergents O. Standard Test Method for Diagonal Tension (Shear)in Masonry Assemblages.
2. Out-of-plane strengthening of unreinforced masonry walls using near surface mounted fibre reinforced polymer strips
3. Diagonal compression tests on masonry walls strengthened with a GFRP mesh reinforced mortar coating
4. GB/T 8077 (2012) Methods for testing uniformity of concrete admixture.
5. GB/T 2419 (2005) Test method for fluidity of cement mortar.
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献