Abstract

In spite of their drawbacks, rheometers are usually run under isothermal conditions for the cure of rubbers: At least three experiments are needed at different temperatures selected within a narrow temperature window to determine the kinetic parameters of the cure of rubbers, and it takes some time for thermal equilibrium between the sample, initially at room temperature, and the dies to be established. With the rheometer in scanning mode, the dies and the sample are heated from room temperature up to the selected final temperature at a constant rate. The heating rate is crucial in this new method. The rubber used in this study is an ethylene propylene diene monomer vulcanised with 20% sulphur and with a rather high cure enthalpy. The state-of-cure versus temperature curves obtained in scanning mode have been calculated using a numerical model that takes into account the heat transfer by conduction through the rubber, the coefficient of heat transfer at the die-rubber interface, and the kinetics of the heat generated by the cure reaction. The kinetic parameters were determined mathematically from these state-of-cure versus temperature curves, which are similar to torque-temperature curves, by obtaining straight lines from them or using a least squares method. The kinetic parameters calculated in these ways were similar to those introduced by obtaining the state-of-cure versus temperature curves using the numerical model. Whatever the heating rate, ranging from 2 to 10 K/min, and whatever the coefficient of heat transfer at the die-rubber interface which expresses the quality of the contact, the moving die rheometer can be used in scanning mode to determine the kinetics of the cure of rubbers, even when the enthalpy of cure is high.

Publisher

SAGE Publications

Subject

Materials Chemistry,Polymers and Plastics,Ceramics and Composites

Reference22 articles.

1. BrazierD. W.; GrassieN. editor. ‘Developments in Polymer Degradation’; Applied Science, London, vol. 2 (1987), 27.

2. Cure of Thermosetting Resins

Cited by 4 articles. 订阅此论文施引文献 订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献

1. Kinetics of Formation and Degradation of Elastomeric Matrices by a New Generation of Non-ASTM Carbon Blacks;Journal of Research in Science and Engineering;2024-07-28

2. Heat transfer—A review of 2004 literature;International Journal of Heat and Mass Transfer;2010-10

3. Kinetics of the Cure Reaction;Rubber Curing and Properties;2008-12-05

4. A study of heat transfer during molding of elastomers;Chemical Engineering Science;2008-06

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3