Many metallic components, such as retorts in heat treat furnaces, furnace heater tubes and coils in chemical and petrochemical plants, waterwalls and reheater tubes in boilers, and combustors and transition ducts in gas turbines, are subject to oxidation. This chapter explains how oxidation affects a wide range of engineering alloys from carbon and Cr-Mo steels to superalloys. It discusses the kinetics and thermodynamics involved in the formation of oxides and the effect of surface and bulk chemistry. It provides oxidation data for numerous alloys and intermetallics in terms of weight gain, metal loss, depth of attack, and oxidation rate. It also discusses the effect of metallurgical and environmental factors such as oxygen concentration, high-velocity combustion gas streams, chromium depletion and breakaway, component thickness, and water vapor.