Abstract
Abstract
This article focuses on the frequently encountered causes of induction coil failures and typical failure modes in fabrication of hardening inductors, tooth-by-tooth gear-hardening inductors, clamshell inductors, contactless inductors, split-return inductors, butterfly inductors, and inductors for heating internal surfaces. It discusses the current density distribution and the skin effect, the proximity effect, and crack-propagation specifics. The article also describes selected properties of copper alloys, the electromagnetic edge effect of coil copper turn, and the effect of magnetic flux concentrators on coil life. It also reviews the importance of having appropriate and reliable electrical contacts.
Reference44 articles.
1. Elements of Induction Heating
2. Systematic Analysis of Induction Coil Failures and Prevention, Part 1: Introduction;Rudnev;Heat Treat. Prog.,2005
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献
1. Electrically Heated Fluidized Beds─A Review;Industrial & Engineering Chemistry Research;2024-03-04
2. Induction Hardening;Encyclopedia of Iron, Steel, and Their Alloys;2016-01-13
3. Induction Coil Design and Fabrication;Practical Induction Heat Treating;2015-08-01