Abstract
Abstract
The mechanism of contact fatigue can be understood in terms of several sources of stress concentration, or stress raisers, within the macroscopic Hertzian stress field. This article focuses primarily on rolling contact fatigue of hardened bearing steels. It discusses Hertzian shear stresses at and below the contact surfaces and briefly summarizes bearings and gear characteristics. The article provides an overview of the key types of gear and bearing steels. It analyzes two types of macropitting that result from the subsurface growth of fatigue cracks, namely, subsurface-origin macropitting and surface-origin macropitting. The article describes the factors influencing contact fatigue life of hardened steel bearings and gears, including hardness, inclusions, carbides, and residual stresses.
Reference69 articles.
1. Dynamic Capacity of Rolling Bearings;Lundberg;Acta Polytech.,1947
Cited by
14 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献
1. Dark etching regions under rolling contact fatigue: a review;Materials Science and Technology;2021-03-04
2. Rolling-Contact Fatigue;Failure Analysis and Prevention;2021-01-15
3. Fatigue Failures;Failure Analysis and Prevention;2021-01-15
4. Metallographic Techniques in Failure Analysis[1];Failure Analysis and Prevention;2021-01-15
5. Friction and Wear of Rolling-Element Bearings;Friction, Lubrication, and Wear Technology;2017-12-31