Impact of X-rays on fission fragments track etch parameters in Lexan detector as analyzed by FTIR spectroscopy

Author:

Kumar Ashok1ORCID,Singh M. K.2,Jain R. K.3

Affiliation:

1. Physics Department, Shaheed Rajguru College of Applied Sciences for Women, University of Delhi, New Delhi 110096, India

2. Department of Physics, Institute of Sciences and Humanities, G. L. A. University, Mathura 281406, Uttar Pradesh, India

3. Department of Physics, Shobhit Institute of Engineering, and Technology (Deemed to-be-University), Meerut 250110, Uttar Pradesh, India

Abstract

Irradiation effects of X-rays (45 min and 90 min) on track etch parameters of Lexan polycarbonate detectors have been studied with respect to structural behavior using Fourier transform infrared spectroscopy (FTIR) spectroscopy. Pre-exposure and post-exposure of X-rays bring significant changes in track etch parameters (bulk etch rate (BER) and track etch rate (TER)) of Lexan polycarbonate detectors at 55[Formula: see text]C to 75[Formula: see text]C. The energy carried by X-rays results in hardening due to cross-linkage and softening due to chain scission of Lexan polycarbonate detectors. BERs and TERs follow Arrhenius equations, and slopes of graph reveal information about activation energy of BERs and TERs. Bulk activation energies calculated are found to be 0.91 eV (unexposed), 0.94 eV (pre-exposed 45 min), 0.96 eV (pre-exposed 90 min), 0.88 eV (post-exposed 45 min) and 0.86 eV (post-exposed 90 min) and are also found to be in agreement with available literature. Track activation energies (TAEs) calculated are found to be 0.74 eV (unexposed), 0.75 eV (pre-exposed 45 min), 0.77 eV (pre-exposed 90 min), 0.74 eV (post-exposed 45 min) and 0.73 eV (post-exposed 90 min). Post-exposure of X-rays for 90 min on Lexan polycarbonate detectors results in enhancement of sensitivity and recorded highest (12.72) at 65[Formula: see text]C. The critical angle of Lexan polycarbonate detectors is also affected by post-exposure of X-rays for 90 min and found maximum (38.59[Formula: see text] at 75[Formula: see text]C. FTIR spectra confirm cross-linkage in Lexan polycarbonate detector during 3 h exposure of fission fragments (FFs) of [Formula: see text]Cf as compared to 2 h exposure.

Publisher

World Scientific Pub Co Pte Ltd

Subject

General Physics and Astronomy,Nuclear and High Energy Physics

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3