Abstract
The Cd[Formula: see text]Zn[Formula: see text]O thin films have been deposited on glass and Si substrates at room-temperature with different Cd contents (x = 0, 2%, 4% and 6 wt.%) by pulsed laser deposition (PLD) technique. X-ray diffraction (XRD) analyses evidenced that the films possess polycrystalline and a hexagonal ZnO crystal structure for x = 0, 2% and 4% with a preferred orientation in the a-axis (101) direction, while films with a mixed hexagonal and cubic structure was revealed for x = 6 wt.%. Electrical measurement presented that the resistivity decreased with increased temperature and concentration of Cd. The deliberated activation energy was reduced was from 0.224 to 0.113 eV with increase doping concentration. Current–voltage (I–V) and capacitance–voltage (C–V) characteristics of the fabricated Cd[Formula: see text]Zn[Formula: see text]O/p-Si heterojunction varied with the applied bias and the Cd concentration. The results of the values of built-in potential (V[Formula: see text]) and the ideality factor (n) increased with raising Cd concentration.
Publisher
World Scientific Pub Co Pte Lt
Subject
Condensed Matter Physics,Statistical and Nonlinear Physics
Cited by
17 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献