Introduction The aim of this study was to evaluate the micro-shear bond strength (μSBS) of different repair systems (Clearfil Repair, iGOS Repair) to restorative materials for CAD/CAM (Cerasmart, Lava Ultimate, InCoris TZI , VITA Suprinity, VITA Mark II, IPS e.max CAD, IPS Empress CAD). Methodology The 140 1.2 mm-thick specimens were prepared from CAD/CAM blocks (n=20) and thermocycled (10,000 cycles, 5–55°C, dwell time 20s). The specimens were randomly divided into two groups according to the repair system: Clearfil Repair (40% phosphoric acid+mixture of Clearfil Porcelain Bond Activator and Clearfil SE Bond Primer+Clearfil SE Bond+CLEARFIL MAJESTY ES-2) and iGOS Repair (40% phosphoric acid+ Multi Primer LIQUID+ iGOS Bond+ iGOS Universal). The composite resins were polymerized. All specimens were stored in distilled water at 37°C for 24 hours. The μSBS test was performed with a micro-shear testing machine (at 1 mm/min). The data were analyzed using two-way ANOVA, Tukey’s multiple comparison tests at a significance level of p<0.05. Each failure modes were examined under a stereomicroscope at×16 magnification. Results The type of CAD/CAM restorative material and repair system showed a significant effect on the μSBS (p<0.05). Specimens repaired with the iGOS Repair system showed the highest μSBS values than the Clearfil Repair system among all tested materials except for the InCoris TZI group (p<0.05). Conclusion All groups, except for the InCoris TZI group, repaired with iGOS Repair system showed higher μSBS than Clearfil Repair. The type of restoration and repair material is important in the success of the fracture repair.
Publisher
ROPOSTURO Romanian Association of Oral Rehabilitation and Posturotherapy
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献