Abstract
Results from laboratory experiments are presented on extraction of zinc available in waste from lead-zinc metallurgy, mixed with lead-zinc flotation tailings and some waste rock, by leaching it under atmospheric conditions with sulfuric acid (H2SO4) solutions (5 and 10 wt. %) and 30 % hydrogen peroxide in the temperature range of 25 - 80 °C, at leaching time 30 - 120 min. Material leaching with 10 % H2SO4 solution at 70 °C for one hour brings into pregnant leach solution (PLS) around 80 % of zinc available. Imposing an electrochemical impact during the leaching process increases the quantity of leached zinc by around 5 %. Direct electrowinning from the PLS obtains zinc metal of grade 75-76 %. The suggested treatment removes metals-pollutants from accumulated mixed technogenic waste therefore rendering it more environmentally friendly. Experiments showed that old mixed waste from mining, mineral processing and metallurgy activities merits further studies as secondary source of metals.
Reference31 articles.
1. U. S. Geological Survey, Mineral commodity summaries 2021 (U. S. Geological Survey, 2021)
2. European Commission, Study on the EU’s list of Critical Raw Materials (2020), Factsheets on Non-critical Raw Materials, (Publications Office of the European Union, Luxembourg, 2020)
3. Study on the improvement of the zinc pressure leaching process
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献