Root cause analysis of the Circular hole corrosion failure of N80 tubing

Author:

Zhang Shuxin,Yan Xi,Ma Chunli,Feng Jie,Wang Shuai

Abstract

During well repair operations in an oil field, a Φ73.02 mm×5.51 mm N80 grade flat oil pipe with a circular hole was found. The depth of the well is between 550 meters to 2100 meters, with a usage cycle of 120 days. In order to figure out the root cause of the circular hole failure, a series of experiments were carried out. The chemical composition, yield strength, tensile strength, and elongation of the oil pipe meet the requirements of API SPEC 5CT-2018 standard. The microstructure of the oil pipe matrix consists of ferrite and pearlite, and there are no obvious cracks. The grain size of the material is all above 8.5 levels, and there are no coarse grains or non-metallic inclusions exceeding the standard. The perforation of the oil pipe is caused by internal corrosion, mainly due to CO2 corrosion and dissolved oxygen corrosion. The coexistence of Ca2+ and Mg2+ ions, iron bacteria, and corrosive bacteria in the wellbore fluid can lead to scale deposition inside the pipe, causing under-deposit corrosion, and the accelerating effect of Cl ions on corrosion ultimately leads to perforation of the pipe.

Publisher

EDP Sciences

Subject

General Medicine

同舟云学术

1.学者识别学者识别

2.学术分析学术分析

3.人才评估人才评估

"同舟云学术"是以全球学者为主线,采集、加工和组织学术论文而形成的新型学术文献查询和分析系统,可以对全球学者进行文献检索和人才价值评估。用户可以通过关注某些学科领域的顶尖人物而持续追踪该领域的学科进展和研究前沿。经过近期的数据扩容,当前同舟云学术共收录了国内外主流学术期刊6万余种,收集的期刊论文及会议论文总量共计约1.5亿篇,并以每天添加12000余篇中外论文的速度递增。我们也可以为用户提供个性化、定制化的学者数据。欢迎来电咨询!咨询电话:010-8811{复制后删除}0370

www.globalauthorid.com

TOP

Copyright © 2019-2024 北京同舟云网络信息技术有限公司
京公网安备11010802033243号  京ICP备18003416号-3