Nikitin Pavel,Zhukov Ilya,Platov Vladimir
Abstract
In work studies of phase composition, hardness and density of materials based on AlMgB14 synthesized by hot pressing method at temperatures of 1300 and 1400 °C under pressure 50 MPa from aluminum, magnesium and boron powders (E1 mixture), as well as from original powder of aluminum-magnesium alloy (E2 mixture) were conducted. AlMgB14 phase content of obtained bulk samples is ~ 95 wt. %. The maximum hardness of 14GPa and density of 2.1 g/cm3, respectively, has a sample, marked as E1, synthesized at a temperature of 1400 °C.