Author:
Tretyakov Dmitry,Belyaev Alexander,Galyautdinova Aliya,Polyanskiy Vladimir,Strekalovskaya Darya
Abstract
The paper presents the results of investigation of acoustic anisotropy in industrial alloy made of steel 14HGNDC after hydrogen-induced cracking (HIC) tests according to the standard NACE TM0284-2003. It was found that location and parameters of corrosion cracks with size about 20 microns can be determined by distribution and value of acoustic anisotropy. A quantitative relationship between value of acoustic anisotropy and size of corrosion cracks in the range from 60 to 6600 microns was established. The obtained results have a great importance for improving methods of hydrogen-induced cracking tests and for non-destructive testing of brittle destruction of structures in oil and gas industry by using the acoustodamage method.
Cited by
5 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献