Abstract
Cyclic heterogeneous deformation, slip characteristics and crack nucleation with different microstructures, such as bimodal microstructure (BM) and fine lamellar microstructure (FLM) in TC21 alloy (Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb-0.1Si), were systematically investigated and analyzed during high cycle fatigue at room temperature. The results demonstrated that the FLM microstructure possesses higher high-cycle fatigue strength than those of the BM one. For BM, the heterogeneous plastic deformation existed within the different large primary α phase, such as equiaxed primary α and primary α lath. The cracks at interfaces and slip bands easily coalesce with each other to form large cracks in BM. However, the α laths with similar morphology and size (nanosize) distributed uniformly in FLM and could relatively deform homogeneously in micro-region, which delayed the initiation of the fatigue crack. Based on the electron-backscattered diffraction (EBSD) analysis, it found that the strain was nonuniformly distributed in BM, however, it is relatively homogeneous in FLM. Moreover, lots of straight cracks are parallel and along single intrusions within the β grain which delays the coalescence of cracks.
Reference33 articles.
1. Leyens C., Peters M., Titanium and titanium alloys: fundamentals and applications, John Wiley & Sons. (2003)
2. Banerjee D., Williams J.C.. Acta Mater. 61(3) (2013)
3. Lütjering G., Williams J.C.. Titanium, Berlin: Springer. (2003)
4. Zhao Y.Q., Yang G.J.. Titanium Industry Progress. 23(5) (2006)
5. Wang X.N., Zhu Z.S., Tong L., Zhou Y., Zhou X.H., Yu H.Q.. Rare Metals Letters.27 (2008)
Cited by
2 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献