Author:
Vaško Milan,Baniari Vladislav,Handrik Marián,Vaško Alan,Jakubovičová Lenka,Kopas Peter
Abstract
The main idea of this paper is to compare the results of FE analysis and data obtained by experiment for identification of residual stresses in welded high-strength steels. The DOMEX steels welded by two technologies are compared – steel welded with laser beam and steel welded by electric arc. Residual stresses at the surface and just below the surface were evaluated using X-rays at predefined points. These data were subsequently processed in MATLAB and evaluated. FE analyzes were performed in software SYSWELD and ADINA.