Al-Zn-Mg-Cu alloy containing 2%Mn was made using spray forming method and hot
extrusion. XRD, OM, and SEM were used to investigate the microstructure. Results showed that after
being hot extruded and solid solution treated, the Al alloy matrix had uniformly fine recrystallized
grain with an average size of 8μm. The particles of MnAl6 were formed during the spray forming
process and distributed along the grain boundary. Deformation and spheroidization of MnAl6
particles were occurred during post hot extrusion and solid solution treament, which would be benefit
to the improvement of toughness of Al alloy. When aged at the T6 conditions, the tensile strength of
the Al alloy was increased up to 775MPa with the elongation of 4.3%, the fracture surface consisted
mainly of dimples with a size lower than 500nm.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Reference11 articles.
1. P. Lengsfeld, J.A. Juarez-Islas, W.A. Cassada, et al: Inter J Rapid Solid Vol. 8 (1995), p.237.
2. S.G. Lim, M. Sunamat, J. Kaneko: J Jpn Inst Light Metals Vol. 41 (1991), p.440.
3. J. Kusui, T. Yokte, K. Osamura, et al: Mater Sci Forum Vol. 217-222 (1996), p.1823.
4. K. Osamura, K. Kohno, H. Okuda, et al: Mater Sci Forum Vol. 217-222 (1996), p.1823.
5. J. Chang, I. Moon, C. Choi: Metall Mater Trans. A Vol. 29 (1998), p.1873.
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献