The characteristics of Ni-Cr porous alloys containing 0.5 wt%Cr up to 12 wt%Cr were determined. The alloys were prepared from a mix of Ni-particles with filamentary shape and Cr-particles with irregular shape which then mixed with 0.5 wt% paraffin wax as a binder. The samples were formed by compaction and then sintered at 1200 °C for 1 h. The microstructure of samples was found to consist of a Ni-Cr solid solution matrix with X-ray energy dispersive analysis of Cr% less than 0.33 wt%. The matrix microstructure which composed of equiaxed grains (20-60 μm) surrounded high Cr content islands which also contained γ phase (Ni2.88 Cr1.22). The apparent density of the alloys was found to decrease with Cr content from 8.32 g/cm3 for samples containing 0.5 wt%Cr to 7.26 g/cm3 for samples containing 12 wt%Cr. Therefore, the estimated porosity was found to increase from 6.4% to 16.6% with increasing Cr content from 0.5 wt% to 12 wt%. The microhardness of the samples varied from 153.6 to 284.2 VHN for the equiaxed grains and from 119.6 to 240.6 VHN for the island areas.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,General Materials Science
Reference30 articles.
1. V. Coman, B. Robotin, P. Ilea, Nickel recovery/removal from industrial wastes: A review, Resources, Conservation and Recycling, 73 (2013) 229-238.
2. X. Maoquan, High temperature oxidation and wear behavior of powder metallurgically developed Ni-Cr-W-Al-Ti-MoS2 composite" Indian J Eng Mater Sci, 16 (2009) 111-115.
3. L.Z. Mohamed, W.A. Ghanem, O.A. El Kady, M.M. Lotfy, H.A. Ahmed, F.A. Elrefaie, Oxidation characteristics of porous-nickel prepared by powder metallurgy and cast-nickel at 1273 K in air for total oxidation time of 100 h, J Adv. Res.(JAR), 8 (2017) 717–729.
4. L.Z. Mohamed, W.A. Ghanem, O.A. El Kady, M.M. Lotfy, H.A. Ahmed, F.A. Elrefaie, Oxidation characteristics of porous nickel low-chromium binary alloys in air at 1273K for 100 h, KEM, 786 (2018) 37-43.
5. C.H. Zhou, R.Y. Pan, H. Zhang, X.G. Guan, Oxidation behavior of Ni-10Cr alloy under the compressive stress at 900 ℃, 3rd Asia-Pacific Electronics and Electrical Eng. Conf. (EEEC 2018), (2018).
Cited by
9 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献