Abstract
In this study, effect of thermal cycling after water absorption on flexural property of CFRP(Carbon Fiber Reinforced Plastics) was examined. Water absorption tests were conducted for 24 hours, 100 hours and 500 hours at 90°C. Thermal cycling test was conducted by using water absorbed specimen. The temperature range of thermal cycling test was from room temperature to-196°C. The static three-point flexural test of CFRP with freezing after water absorption was conducted based on JIS(Japanese Industrial standard) K 7074. Following conclusions are obtained. In case of immersion for 24 hours, flexural strength and modulus of CFRP with freezing after water absorption decreased with an increase of the number of cycles. In case of immersion for 100 hours and 500 hours, flexural strength and modulus of CFRP with freezing after water absorption did not change. The water absorption of CFRP was the phenomenon that the water penetrated into fiber/resin interface. So, in the case of immersion for 24 hours that the absorption time is not so long, damage progresses gradually in thermal cycling test. On the other hand, in the case of immersion for 500 hours is long, the damage progresses at the early stage of the thermal cycling test, and after that the damage does not almost progress.
Publisher
Trans Tech Publications, Ltd.
Reference5 articles.
1. Y. Morino, Cryogenic CFRP propellant tank for reusable launch vehicle, Trans. JSME Annual Meeting (Ⅶ), (2001) 274-275 (in Japanese).
2. T. Gomez-del Rio, R. Zaera, E. Barbero and C. Navarro, Damage in CFRPs due to low velocity impact at low temperature, Compos. Part B, 36 (2005) 41-50.
3. K. Komai, K. Minoshima and N. Ishikawa, Cryogenic temperature and water absorption effect on mechanical properties and fatigue strength of carbon fiber reinforced plastics, Trans. JSME, 59 (1993) 1677-1683, (in Japanese).
4. T. Takagi, T. tuji, K. Takahashi, H. Oguma and K. Nakamura, Effect of aqueous environment on mechanical properties of carbon fiber reinforced plastics, Trans. JSME Hokkaido Branch, 47 (1993), 163-170.
5. H. Katoh, Durability of carbon fiber/epoxy resin plastics after thermal cycling, Proc. 38th Symp. Compos. Mater., 38 (2013), 163-164 (in Japanese).
Cited by
1 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献