Abstract
The effect of heating cycles of polyether ether ketone up to 420 °C on the thermophysical properties was studied by the method of differential-scanning calorimetry. It is shown that with each subsequent heating the glass transition temperature increases, while the melting and crystallization temperature decreases, which may indicate an increase in the molecular weight of the polymer due to the structuring processes. The main degradation products of polyether ether ketone in air at temperatures of 350-450 °C were determined by gas chromatography and thermal decomposition schemes were proposed.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Reference4 articles.
1. Shakhmurzova K.T., Kurdanova Zh.I., Khashirova S.Yu., Beev A.A., Pahomov S.I., Ligidov M.Kh., Mikitaev A.K., Polyether ketones. Production, properties and application, Proceedings of high schools. Chemistry and Chemistry. technology. Izvestiya vuzov. Khimiya i khim. tekhnologiya. 58 (2015).
2. A.A. Zhansitov, A.L. Slonov, R.A. Shetov, A.E. Baikaziev, K.T. Shakhmurzova, Zh.I. Kurdanova, S.Yu. Khashirova. Synthesis and properties of polyether ether ketones for 3D printing. Fibre Chemistry 49 (2018) 414-419.
3. A.S. Shabaev, A.A. Zhansitov, Zh.I. Kurdanova, S.Yu. Khashirova, A.K. Mikitaev, New Method of Investigation of Polysulfone Thermal Destruction, Polymer Science, Series B. 59 (2017) 216–224.
4. A.S. Shabaev, A.A. Zhansitov, Z.I. Kurdanova, L.Kh. Kuchmenova, S.Yu. Khashirova, Investigation of thermal and thermo-oxidative degradation of poly(ether ether ketone) by gas chromatography, Chinese Journal of Chromatography. 36 (2018) 395-399.
Cited by
3 articles.
订阅此论文施引文献
订阅此论文施引文献,注册后可以免费订阅5篇论文的施引文献,订阅后可以查看论文全部施引文献