Abstract
Ti alloys are attractive materials for such applications, they are expensive due to the costly alloying elements such as Nb or Mo. The present authors have adopted Mn as a low-cost alloying element, and melted Ti-7, 7.5 and 8 mass%Mn-1.5 and 3mass%Al alloys using a laboratory-scale arc furnace. All specimens prepared from bottom ingots were heat treated at 1223 K for 3.6 ks and quenched in ice water. In the 7 and 7.5Mn-Al alloys, the β phase and orthorhombic martensite were identified using X-ray diffraction. In the 8Mn-Al alloys, only the β phase was identified. In the 7, 7.5, and 8Mn-Al alloys, the electrical resistivity at room and liquid nitrogen temperature increased with increasing Al content due to dissolution of Al into the β phase, whereas the Vickers hardness decreased with increasing Al content due to decreasing formation of athermal omega by the addition of Al. Heat treatment at 673 K for 60 s almost completely returned deformed Ti-7 and 7.5Mn-3Al specimens to their original shapes, and heat treatment at 773 K for 60 s almost returned deformed Ti-8Mn-Al specimens to their original shapes.
Publisher
Trans Tech Publications, Ltd.
Subject
Mechanical Engineering,Mechanics of Materials,Condensed Matter Physics,General Materials Science
Reference6 articles.
1. Materials Properties Handbook, Titanium Alloys, Eds. R. Boyer, G. Welsch and E. W. Collings, ASM International, Materials Park, Ohio, 1994, P. 3-4.
2. C. Baker, The Shape-Memory Effect in a Titanium –35wt% Niobium Alloy. Metal Science Journal, Vol. 5, 1971, P.92-101.
3. M. Ikeda, D. Sugano, S. Masuda and M. Ogawa, The Influence of Aluminum Content on Shape Memory Effect of Ti-7Cr-Al Alloys Fabricated Using Low Grade Sponge Titanium, Vol. 46, 2005, P. 1604-1609.
4. M. Ikeda, M. Ueda, R. Matsunaga, M, Ogawa and M. Niinomi, Isothermal Aging Behavior of Beta Titanium-Manganese Alloys, Vol. 50, 2009, P. 2737-2743.
5. Y. Takemoto, M. Ochi, T. Senuma, J. Takada, I. Shimizu and K. Matsugi, Unprecedented Phenomena with Tempering of Ti-4Fe-7Al Alloy, J. Japan Inst. Metals, Vol. 76, 2012, P. 449-455.